After taking precise measurements specimen thickness, placed between two parallel plates of the machine, followed by a rate of 60 per minute, 50% compression specimen thickness, so 80,000 times in a row after repeated compression, remove the specimen after 30 minutes on standing, and then measuring the thickness, the rate of compression is obtained.